{"product_id":"fsx414lc-cobalt-superalloy-certified-reference-material-bsfsx414","title":"FSX414LC Cobalt Superalloy Certified Reference Material","description":"\u003cp class=\"font-claude-response-body break-words whitespace-normal\"\u003eThis \u003cstrong\u003eFSX414LC certified reference material\u003c\/strong\u003e is a cobalt-chromium-tungsten-nickel superalloy used as a standard for calibrating and verifying your spectrometer (handheld XRF, handheld LIBS, benchtop XRF, OES). This material is certified with values established through interlaboratory testing, giving you traceable, defensible composition data for calibration checks, instrument verification, and quality control on FSX414LC and other cobalt-based superalloys.\u003c\/p\u003e\n\u003ch2 class=\"font-claude-response-body break-words whitespace-normal\"\u003eFSX414LC Certified Chemical Composition\u003c\/h2\u003e\n\u003cdiv class=\"overflow-x-auto w-full px-2 mb-6\"\u003e\n\u003ctable class=\"min-w-full border-collapse text-sm leading-[1.7] whitespace-normal\"\u003e\n\u003cthead class=\"text-left\"\u003e\n\u003ctr\u003e\n\u003cth scope=\"col\" class=\"text-text-100 border-b-0.5 border-[hsl(var(--border-300)\/0.6)] py-2 pr-4 align-top font-bold\"\u003eElement\u003c\/th\u003e\n\u003cth scope=\"col\" class=\"text-text-100 border-b-0.5 border-[hsl(var(--border-300)\/0.6)] py-2 pr-4 align-top font-bold\"\u003eCertified Value (wt%)\u003c\/th\u003e\n\u003c\/tr\u003e\n\u003c\/thead\u003e\n\u003ctbody\u003e\n\u003ctr\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003eCo\u003c\/td\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003e50.6%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003eCr\u003c\/td\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003e29.7%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003eW\u003c\/td\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003e7.3%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003eNi\u003c\/td\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003e10.4%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003eSi\u003c\/td\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003e0.78%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003eMn\u003c\/td\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003e0.78%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003eC\u003c\/td\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003e0.127%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003eFe\u003c\/td\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003e0.05%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003eN\u003c\/td\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003e0.0027%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003eS\u003c\/td\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003e0.0010%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003eO\u003c\/td\u003e\n\u003ctd class=\"border-b-0.5 border-[hsl(var(--border-300)\/0.3)] py-2 pr-4 align-top\"\u003e0.0008%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003c\/tbody\u003e\n\u003c\/table\u003e\n\u003c\/div\u003e\n\u003cp class=\"font-claude-response-body break-words whitespace-normal\"\u003e\u003ca href=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0591\/2671\/0411\/files\/bsfsx414.pdf?v=1784224737\" title=\"Certificate of Analysis\"\u003eFSX414LC Certificate of Analysis (BS FSX414LC)\u003c\/a\u003e\u003c\/p\u003e\n\u003ch2 class=\"font-claude-response-body break-words whitespace-normal\"\u003eOther Names\u003c\/h2\u003e\n\u003cp class=\"font-claude-response-body break-words whitespace-normal\"\u003eFSX414LC, FSX-414LC, FSX 414LC, FSX414, FSX-414, Cobalt Alloy FSX414LC, Cobalt Superalloy FSX414LC\u003c\/p\u003e\n\u003ch2 class=\"font-claude-response-body break-words whitespace-normal\"\u003eAvailable material forms\u003c\/h2\u003e\n\u003cul class=\"[li_\u0026amp;]:mb-0 [li_\u0026amp;]:mt-1 [li_\u0026amp;]:gap-1 [\u0026amp;:not(:last-child)_ul]:pb-1 [\u0026amp;:not(:last-child)_ol]:pb-1 list-disc flex flex-col gap-1 pl-8 mb-3\"\u003e\n\u003cli class=\"font-claude-response-body whitespace-normal break-words pl-2\"\u003eXRF - Disc: 41mm D x 7mm\u003c\/li\u003e\n\u003cli class=\"font-claude-response-body whitespace-normal break-words pl-2\"\u003eOES - Disc: 41mm D x 19mm\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp class=\"MsoNormal\"\u003eFor questions about sample dimensions or other product details, please \u003ca href=\"https:\/\/alloygeek.com\/pages\/contact\"\u003econtact us\u003c\/a\u003e.\u003c\/p\u003e","brand":"Brammer Standard Company, Inc.","offers":[{"title":"XRF - Disc: 41mm D x 7mm","offer_id":48597491875979,"sku":"AG-BSFSX414-XRF","price":395.0,"currency_code":"USD","in_stock":true},{"title":"OES - Disc: 41mm D x 19mm","offer_id":48597491843211,"sku":"AG-BSFSX414-OES","price":795.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0591\/2671\/0411\/files\/Stainless_Steel_Low_Alloy_Steel_Nickel_Cobalt_Certified_Reference_Material_v2.3.1.jpg?v=1730816111","url":"https:\/\/alloygeek.com\/products\/fsx414lc-cobalt-superalloy-certified-reference-material-bsfsx414","provider":"Alloy Geek","version":"1.0","type":"link"}